Measling

Description:
Destruction (white spots) of the weave interior. These defects are tolerated in general, as long as they do not appear frequently and do not touch two neighbouring conductors or soldering eyes.

Causes/Remedy:

  • resin content in lamination process too low
  • mechanical stress

Zerrütungen innerhalb des Gewebes einer Leiterplatte Source:
visual, optical inspection - general view
Do you have problems with measling ?